How to Choose Rubber Antioxidant?
2026-11-17
The selection of antioxidants should be based on an evaluation of five factors: type of rubber, ageing environment, appearance requirements, migration risk, and validation methods.

How to Select Rubber Antioxidant?
Adhesive Type
Rubber Type / System | Main Ageing Sensitivity Points | Key Points for Antioxidant Selection |
|---|---|---|
Natural Rubber (NR) | Thermal oxygen, ozone, flex fatigue | Amine antioxidants, protective wax; auxiliary antioxidant system when needed |
Styrene Butadiene Rubber (SBR) | Thermal oxygen, ozone, dynamic cracking | p-Phenylenediamines, quinolines, and compounds with protective wax |
Polybutadiene Rubber (BR) | Ozone, flex fatigue, thermal oxygen | Anti-ozonant and dynamic fatigue protection system |
Nitrile Butadiene Rubber (NBR) | Thermal oxygen, extraction in oil medium, metal contact | Thermal oxygen-resistant antioxidants, low-extraction protection system, metal passivation design |
Ethylene Propylene Diene Monomer (EPDM) | Heat, light, long-term outdoor exposure | Phenolic antioxidants, auxiliary antioxidants, weather-resistant protection system |
Speciality Rubbers (Silicone Rubber, Fluororubber, etc.) | High temperature, media and special working conditions | Verified by custom formula, processing method and application specification |
Used Environment
Application Scenario | Main Failure Risks | Key Selection Criteria |
|---|---|---|
Tire Sidewall | Ozone cracking, flex fatigue, outdoor ageing | p-Phenylenediamine antiozonants, antioxidant RD, blended with protective wax |
Rubber Hoses | Thermal oxidation, ozone, medium extraction, dynamic deformation | Amine or phenolic systems; verify medium extraction resistance |
Conveyor Belts & Power Transmission Belts | Flex fatigue, thermal oxidative ageing, crack propagation | Anti-flex antioxidants, synergistic filler and vulcanisation system |
O-rings / Seals | Compression set, thermal oxidation, oil media | Low-extraction, low-migration protection system compatible with media |
Cable & Wire Sheath | Thermal oxidation, copper-catalysed degradation, weather resistance, electrical properties | Heterocyclic, phenolic and auxiliary antioxidant systems |
White or Light-Coloured Rubber | Discolouration, staining, thermal oxidative ageing | Non-staining system: phenolics, heterocyclics, phosphites |
Medical or Food-Contact Rubber | Migration, odour, toxicology and regulatory compliance | Low-migration, low-extraction antioxidants with clear compliance documentation |
Appearance and Contact Requirements
For dark rubber, high-efficacy amine-based antioxidants should be prioritised. For white, light-coloured, transparent, medical, food-contact, or electronic-contact products, priority should be given to protective systems characterised by low contamination, low migration, and low odour.
If rubber products are to be subsequently bonded, coated, printed, or vulcanised, particular attention should be paid to the surface migration of antioxidants and protective waxes. Excessive migration can lead to failure in bonding, pinholes in the coating, whitening on the surface, or contamination in contact.
Migration and Extraction
Antioxidants must migrate to a certain extent to protect the rubber surface; however, excessive migration can lead to blooming, contact contamination, and environmental release. Oils, water, solvents, and cleaning agents can leach out antioxidants, thereby reducing long-term protection. Therefore, migration and leaching should be taken into consideration when evaluating seals, tubes, medical-grade rubber, and rubber for outdoor use.
Common Misconceptions About the Use of Rubber Antioxidants
1. Excessive use of anti-ageing agents (antioxidants/antiozonants) can lead to issues such as blooming (exudation), colour changes, increased odour, contact staining, reduced adhesion, and higher costs. In the case of migrating antiozonants, an insufficient dosage results in inadequate surface protection, while an excessive dosage can cause the agent to migrate to the surface and subsequently precipitate there.
2. Thermo-oxidative ageing, ozone cracking, flex fatigue, metal-catalysed ageing, and extraction through contact with external agents represent distinct failure mechanisms. Different types of rubber products—such as dark-coloured dynamic components, light-coloured items, seals, cable sheaths, or products intended for food contact—require different protection strategies; therefore, the same formulation of anti-ageing agents cannot be applied universally.
3. The failure of rubber products does not necessarily manifest, in the first instance, as a decrease in tensile strength. Other signs may appear early on, such as ozone cracking, an increase in hardness, a reduction in elongation at break, surface blooming, colour changes, swelling due to exposure to external agents, or a loss of adhesion. The evaluation of anti-ageing agents must be based on performance indicators relevant to the specific end-use of the product.
4. The compatibility of anti-ageing agents varies depending on the vulcanisation system employed (sulphur-based, peroxide-based, or resin-based). Some anti-ageing agents, by acting as free-radical scavengers, can interfere with the efficiency of peroxide crosslinking; consequently, it is essential to evaluate vulcanisation curves, crosslink density, initial physical properties, and performance after ageing.